ASTM D 1675 : 2018
Current
The latest, up-to-date edition.
Hardcopy , PDF
English
01-05-2018
1.1These test methods cover procedures for testing polytetrafluoroethylene tubing for use as electrical insulation. The procedures appear in the following sections:
| | ASTM |
Conditioning | 7 | ... |
Dielectric Breakdown Voltage | 28 – 30 | D149, D876 |
Inside Diameter | 8 – 13 | D876 |
Mandrel Bend Test | 46 – 52 | D149, D876 |
Melting Point | 41 – 45 | D3418, D4895 |
Penetration Test | 26 and 27 | D876 |
Specific Gravity | 36 – 40 | D792, D1505 |
Strain Relief | 31 – 35 | ... |
Volatile Loss | 20 – 25 | ... |
Wall Thickness | 14 – 19 | ... |
Note 1:These test methods are similar but not identical to those in IEC 60684–2.
1.2The values stated in inch-pound units are the standard except for temperature, which is stated in degrees Celsius. Values in parentheses are for information only.
1.3This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use. For specific warning statements, see Section 5.
1.4This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.