PROCEDURE FOR GTAW OF 625 ALLOY TO 300 SERIES STAINLESS STEEL
01-01-2014
1.0 PURPOSE
2.0 APPLICABILITY
3.0 REFERENCES AND APPLICABLE DOCUMENTS
4.0 RESPONSIBILITIES
5.0 REQUIREMENTS AND PROCEDURES
6.0 RECORDS AND FORMS
7.0 ABBREVIATIONS AND ACRONYMS
8.0 ATTACHMENTS
Specifies a qualified American Society of Mechanical Engineers (ASME) weld procedure for Gas Tungsten Arc Welding (GTAW) of 625 Alloy (UNS N06625) to 300 Series Stainless Steel at SSC.
Committee |
WELD
|
DocumentType |
Standard
|
PublisherName |
National Aeronautics and Space Administration
|
Status |
Current
|
SAE AMS 5896 : 2015 | STEEL, CORROSION AND HEAT-RESISTANT, SEAMLESS OR WELDED HYDRAULIC TUBING, 18.5CR - 10.5NI - 0.55TI (321), SOLUTION HEAT TREATED AND COLD DRAWN, 1/8 HARD TEMPER |
SAE AMS 5645 : 2016 | STEEL, CORROSION AND HEAT RESISTANT, BARS, WIRE, FORGINGS, TUBING, AND RINGS, 18CR - 10NI - 0.40TI (321), SOLUTION HEAT TREATED |
SAE AMS 5402 : 2004 | NICKEL ALLOY, CORROSION AND HEAT RESISTANT, INVESTMENT CASTINGS 62NI - 21.5CR - 9.0MO - 3.6CB (NB) AS CAST |
ASTM A 632 : 2004 | Standard Specification for Seamless and Welded Austenitic Stainless Steel Tubing (Small-Diameter) for General Service |
SAE AMS 5912 : 2014 | STEEL, CORROSION-RESISTANT, SHEET AND STRIP, 19CR - 9.2NI (SAE 30304), COLD ROLLED, 3/4 HARD, 175 KSI (1207 MPA) TENSILE STRENGTH |
SAE AMS 5501 : 2002 | STEEL, CORROSION RESISTANT, SHEET, STRIP, AND FOIL, 19CR - 9.5NI (304), COLD ROLLED, 125 KSI (862 MPA) TENSILE STRENGTH |
SAE AMS 5558H : 2016 | STEEL, CORROSION AND HEAT-RESISTANT, WELDED TUBING 18CR - 10.5NI - 0.70CB (NB) (347) THIN WALL SOLUTION HEAT TREATED |
SAE AMS 5910 : 2012 | STEEL, CORROSION-RESISTANT, SHEET, STRIP, AND PLATE, 19CR - 9.2NI (SAE 30304) COLD ROLLED, 125 KSI (862 MPA) TENSILE STRENGTH |
SAE AMS 5581 : 2010 | NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SEAMLESS OR WELDED TUBING, 62NI - 21.5CR - 9.0MO - 3.7CB (NB), ANNEALED |
SAE AMS 5897 : 2012 | STEEL, CORROSION AND HEAT-RESISTANT, SEAMLESS OR WELDED HYDRAULIC TUBING, 18.5CR - 11NI - 0.80CB (NB) (SAE 30347), SOLUTION HEAT TREATED AND COLD DRAWN, 1/8 HARD TEMPER |
ASTM A 908 : 2003 | Standard Specification for Stainless Steel Needle Tubing |
SAE AMS 5599 : 2016 | NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 62NI - 21.5CR - 9.0MO - 3.7 CB (NB), ANNEALED |
SAE AMS 5512 : 2012 | STEEL, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 18CR - 10.5NI - 0.80CB (SAE 30347), SOLUTION HEAT TREATED |
SAE AMS 5571J:2012(R2018) | STEEL, CORROSION AND HEAT-RESISTANT, SEAMLESS TUBING, 18CR - 10.5NI - 0.70CB (NB) (347), SOLUTION HEAT TREATED |
ASTM A 959 : 2016 : REDLINE | Standard Guide for Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels |
ASTM A 666 : 2015 : REDLINE | Standard Specification for Annealed or Cold-Worked Austenitic Stainless Steel Sheet, Strip, Plate, and Flat Bar |
SAE AMS 5573 : 2012 | STEEL, CORROSION AND HEAT-RESISTANT, SEAMLESS TUBING, 17CR - 12NI - 2.5MO (SAE 30316), SOLUTION HEAT TREATED |
SAE AMS 5564 : 2013 | STEEL, CORROSION RESISTANT, TUBING 19CR - 10NI (SAE 30304) HIGH-PRESSURE HYDRAULIC, WELDED PLUS ULTRASONICALLY TESTED OR SEAMLESS COLD DRAWN, ONE EIGHTH - HARD TEMPER |
SAE AMS 5913 : 2014 | STEEL, CORROSION-RESISTANT, SHEET AND STRIP, 19CR - 9.2NI (SAE 30304), COLD ROLLED, FULL HARD, 185 KSI (1276 MPA) TENSILE STRENGTH |
SAE AMS 5563 : 2012 | STEEL, CORROSION RESISTANT, SEAMLESS OR WELDED TUBING, 19CR - 9.5NI (SAE 30304), COLD DRAWN, 1/4 HARD TEMPER |
SAE AMS 5513 : 2015 | STEEL, CORROSION-RESISTANT, SHEET, STRIP, AND PLATE, 19CR - 9.2NI (SAE 30304), SOLUTION HEAT TREATED |
SAE AMS 5647 : 2017 | STEEL, CORROSION-RESISTANT, BARS, WIRE, FORGINGS, MECHANICAL TUBING, AND RINGS, 19CR - 9.5NI, SOLUTION HEAT TREATED |
SAE AMS 5584 : 2012 | STEEL, CORROSION AND HEAT RESISTANT, SEAMLESS AND WELDED HYDRAULIC TUBING, 17CR - 12NI - 1.5MO - 0.03C MAX, COLD DRAWN, 1/8 HARD TEMPER |
SAE AMS 5648 : 2016 | STEEL, CORROSION AND HEAT-RESISTANT, BARS, WIRE, FORGINGS, TUBING, AND RINGS, 17CR - 12NI - 2.5MO (316), SOLUTION HEAT TREATED |
SAE AMS 5654 : 2011 | STEEL, CORROSION AND HEAT RESISTANT, BARS, WIRE, FORGINGS, TUBING, AND RINGS, 18CR - 11NI - 0.60CB (NB) (347), PREMIUM AIRCRAFT QUALITY, CONSUMABLE ELECTRODE MELTED, SOLUTION HEAT TREATED |
SAE J 405 : 1998 | CHEMICAL COMPOSITIONS OF SAE WROUGHT STAINLESS STEELS |
ASTM B 834 : 2017 : REDLINE | Standard Specification for Pressure Consolidated Powder Metallurgy Iron-Nickel-Chromium-Molybdenum (UNS N08367), Nickel-Chromium-Molybdenum-Columbium (Nb) (UNS N06625), Nickel-Chromium-Iron Alloys (UNS N06600 and N06690), and Nickel-Chromium-Iron-Columbium-Molybdenum (UNS N07718) Alloy Pipe Flanges, Fittings, Valves, and Parts |
SAE AMS 5566 : 2011 | STEEL, CORROSION RESISTANT, SEAMLESS OR WELDED HYDRAULIC TUBING, 19CR - 10NI (304) HIGH PRESSURE, COLD DRAWN |
SAE AMS 5567 : 2015 | STEEL, CORROSION RESISTANT, SEAMLESS OR WELDED HYDRAULIC TUBING, 19CR - 10NI (304), SOLUTION HEAT TREATED |
SAE AMS 5510S : 2014 | STEEL, CORROSION AND HEAT-RESISTANT, SHEET, STRIP AND PLATE, 18CR - 10.5NI - 0.40TI (SAE 30321) SOLUTION HEAT TREATED |
ASTM A 511 : 2004 | Standard Specification for Seamless Stainless Steel Mechanical Tubing |
SAE AMS 5869 : 2013 | NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE 62NI - 21.5CR - 9.0MO - 3.7CB SOLUTION HEAT TREATED |
SAE AMS QQ S 763D : 2013(S2015) | STEEL, CORROSION RESISTANT, BARS, WIRE, SHAPES, AND FORGINGS |
SAE AMS 5857 : 2013 | STEEL, CORROSION-RESISTANT, BARS AND WIRE, 19CR - 10NI (304), HIGH YIELD STRENGTH, SOLUTION HEAT TREATED AND COLD WORKED |
SAE AMS 5559 : 2012 | STEEL, CORROSION AND HEAT-RESISTANT, WELDED TUBING, 18CR - 10.5NI - 0.40TI (SAE 30321), THIN WALL, SOLUTION HEAT TREATED |
SAE J 467 : 1968 | SPECIAL PURPOSE ALLOYS ('SUPERALLOYS') |
SAE AMS 5575 : 2013 | STEEL, CORROSION AND HEAT-RESISTANT, WELDED TUBING, 18CR - 10.5NI - 0.70CB (NB) (347), SOLUTION HEAT TREATED |
SAE AMS 5911 : 2014 | STEEL, CORROSION-RESISTANT, SHEET AND STRIP, 19CR - 9.2NI (SAE 30304) COLD ROLLED, 1/2 HARD, 150 KSI (1034 MPA) TENSILE STRENGTH |
ASTM A 965/A965M : 2014-05 | SPECIFICATION FOR STEEL FORGINGS, AUSTENITIC, FOR PRESSURE AND HIGH TEMPERATURE PARTS |
SAE AMS 5570 : 2013 | STEEL, CORROSION AND HEAT-RESISTANT, SEAMLESS TUBING 18CR - 11NI - 0.40TI (321), SOLUTION HEAT TREATED |
MIL-E-21562 Revision E:1989 | ELECTRODES AND RODS - WELDING, BARE, NICKEL ALLOY |
SAE AMS 5639 : 2017 | STEEL, CORROSION-RESISTANT, BARS, WIRE, FORGINGS, MECHANICAL TUBING, AND RINGS, 19CR - 10NI, SOLUTION HEAT TREATED |
ASTM B 705 : 2017 : REDLINE | Standard Specification for Nickel-Alloy (UNS N06625, N06219 and N08825) Welded Pipe |
SAE AMS 5511 : 2013 | STEEL, CORROSION-RESISTANT, SHEET, STRIP, AND PLATE, 19CR - 9.5NI (304L), SOLUTION HEAT TREATED |
MIL-DTL-23196 Revision F:2017 | STEEL PLATE, CORROSION RESISTANT (UNS S30400/S30403, S31600/S31603, S31703, S34700, AND S34800) |
SAE AMS 5907 : 2012 | STEEL, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 17CR - 12NI - 2.5MO (SAE 30316), COLD ROLLED, 1/4 HARD, 125 KSI (862 MPA) TENSILE STRENGTH |
ASTM A 554 : 2016 : REDLINE | Standard Specification for Welded Stainless Steel Mechanical Tubing |
NASA SSTD 8070 0013 : 2015 | CLASSES OF WELDING INSPECTION |
SAE AMS 5524 : 2014 | STEEL, CORROSION AND HEAT-RESISTANT, SHEET, STRIP AND PLATE 18CR - 13NI - 2.5MO (SAE 30316) SOLUTION HEAT TREATED |
NASA SSTD 8070 0005 : 2016 | PREPARATION, REVIEW, APPROVAL, AND RELEASE OF SSC STANDARDS |
NASA SSTD 8070 0014 : 2010 | STANDARD FOR QUALIFYING WELDERS AND WELDING PROCEDURES |
SAE AMS 5653 : 2012 | STEEL, CORROSION AND HEAT-RESISTANT, BARS, WIRE, FORGINGS, TUBING, AND RINGS, 17CR - 12NI - 2.5MO (0.030 MAX C) (316L), SOLUTION HEAT TREATED |
SAE AMS 5666H : 2016 | NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, EXTRUSIONS, AND RINGS, 62NI - 21.5CR - 9.0MO - 3.65CB (NB), ANNEALED |
SAE AMS T 6845 : 2013 | TUBING, STEEL, CORROSION-RESISTANT (S30400), AEROSPACE VEHICLE HYDRAULIC SYSTEM 1/8 HARD CONDITION |
ASTM B 751 : 2008 | Standard Specification for General Requirements for Nickel and Nickel Alloy Welded Tube |
SAE AMS 5868 : 2012 | STEEL, CORROSION-RESISTANT, SEAMLESS AND WELDED AIRCRAFT TUBING, 19CR - 9.5NI (SAE 30304), COLD DRAWN, 1/2 HARD TEMPER |
SAE AMS 5401 : 2004 | NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, INVESTMENT CASTINGS, 62NI - 21.5CR - 9.0MO - 3.6CB (NB), VACUUM MELTED, VACUUM CAST, AS CAST |
SAE AMS 5576 : 2005 | STEEL, CORROSION AND HEAT RESISTANT, WELDED TUBING - 18CR - 10.5NI - 0.40TI (SAE 30321) SOLUTION HEAT TREATED |
SAE AMS 5556 : 2016 | STEEL, CORROSION AND HEAT-RESISTANT, SEAMLESS OR WELDED HYDRAULIC TUBING 18CR - 11NI - 0.70CB (347) SOLUTION HEAT TREATED |
MIL-DTL-23195 Revision F:1997 | STEEL BARS AND FORGINGS, CORROSION RESISTANT, AUSTENITIC (UNS S30400, S30403, S31600, S31603, S34700, AND S34800) |
SAE AMS 5565L : 2013 | STEEL, CORROSION RESISTANT, WELDED TUBING, 19CR - 9.5NI (304), SOLUTION HEAT TREATED |
SAE AMS 5557 : 2012 | STEEL, CORROSION AND HEAT RESISTANT, SEAMLESS OR WELDED HYDRAULIC TUBING, 18.5CR - 10.5NI - 0.40TI (SAE 30321), SOLUTION HEAT TREATED |
SAE AMS 5507 : 2012 | STEEL, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 17CR - 13NI - 2.5MO (316L), SOLUTION HEAT TREATED |
SAE AMS 5560 : 2016 | STEEL, CORROSION RESISTANT, SEAMLESS TUBING, 19CR - 10NI (304), SOLUTION HEAT TREATED |
Access your standards online with a subscription
Features
-
Simple online access to standards, technical information and regulations.
-
Critical updates of standards and customisable alerts and notifications.
-
Multi-user online standards collection: secure, flexible and cost effective.