Wear-resistant white cast iron

Available format(s)

Hardcopy , PDF 1 User , PDF 3 Users , PDF 5 Users , PDF 9 Users

Superseded date

06-30-2017

Language(s)

English

Published date

01-01-2002

1 - AS 2027-2002 WEAR-RESISTANT WHITE CAST IRON
4 - PREFACE
5 - CONTENTS
6 - 1 SCOPE
6 - 2 REFERENCED DOCUMENTS
6 - 3 DEFINITIONS
6 - 3.1 Cast irons
6 - 3.2 White iron
7 - 4 DESIGNATIONS
7 - 4.1 General
7 - 4.2 White cast irons specified by hardness
7 - 4.3 Nickel-chromium type
7 - 4.4 High chromium type
7 - 5 CHEMICAL COMPOSITION
7 - 5.1 General
7 - 5.2 Sampling and analysis
7 - 6 MICROSTRUCTURAL EXAMINATION
10 - 7 HARDNESS
10 - 7.1 Hardness test
10 - 7.2 White cast irons specified by hardness
10 - 7.3 Nickel-chromium type
10 - 7.4 High chromium type
10 - 8 ROUNDING OF TEST RESULTS
10 - 9 INDEPENDENT TESTS
11 - APPENDIX A - HEAT TREATMENT AND MICROSTRUCTURES OF WEAR-RESISTANT WHITE CAST IRONS
11 - A1 WHITE CAST IRON SPECIFIED BY HARDNESS
11 - A1.1 Heat treatment
11 - A1.2 Microstructure
11 - A2 NICKEL-CHROMIUM TYPE
12 - A3 HIGH CHROMIUM TYPE
13 - APPENDIX B - NICKEL-CHROMIUM TYPE-RELATIONSHIP BETWEENSECTION SIZE AND CHEMICAL COMPOSITION

Specifies requirements for specific types of wear-resistant white iron.

This Standard specifies requirements for the following types of wear-resistant white cast iron: (a) White cast iron specified by hardness. (b) Nickel-chromium type. (c) High chromium type. NOTES:1 For advice and recommendations on information to be supplied by the purchaser at the time of enquiry and order, see AS 4738. 2 For information and advice on casting practices, see AS 4738.3 Information on heat treatment and microstructures of white cast irons is given in Appendix A. 4 Information on section size and chemical composition of nickel-chromium white cast irons is given in Appendix B.5 No provision has been made in this Standard for wear testing as wear rates depend on load, velocity, rate of loading, abrasive material, presence of fluids and many other factors which are difficult to reproduce. It is usually found that the testing of wear-resistant materials in their final application is more satisfactory than any smaller scale test. Anything other than a field test must be accepted as a compromise.

Committee
MT-001
DocumentType
Standard
ISBN
0 7337 4945 3
Pages
8
PublisherName
Standards Australia
Status
Superseded
SupersededBy
Supersedes
UnderRevision

First published as AS 2027-1977.Second edition 1985.Third edition 2002. First published as AS 2027-1977. Second edition 1985. Third edition 2002.

AS/NZS 1050.1:1996 Methods for the analysis of iron and steel Sampling iron and steel for chemical analysis
AS 2706-1984 Numerical values - Rounding and interpretation of limiting values
AS 1816.1-2002 Metallic materials - Brinell hardness test Test method (ISO 6506-1:1999, MOD)

AS 1988.1-2006 Welding of ferrous castings - Steel castings
AS/NZS 3800:2005 Electrical equipment for explosive atmospheres - Repair and overhaul
AS 4738.1-2004 Metal castings - Ferrous sand moulded

View more information
US$48.59
Excluding Tax where applicable

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.