• ASTM A 447/A447M : 1993 : R2007

    Superseded A superseded Standard is one, which is fully replaced by another Standard, which is a new edition of the same Standard.
    Add to Watchlist
    This Standard has been added successfully to your Watchlist.
    Please visit My Watchlist to see all standards that you are watching.
    Please log in or to add this standard to your Watchlist.
    We could not add this standard to your Watchlist.
    Please retry or contact support for assistance.
    We could not add this standard to your Watchlist.
    Please retry or contact support for assistance.
    You have already added this standard to your Watchlist.
    Visit My Watchlist to view the full list.

    Standard Specification for Steel Castings, Chromium-Nickel-Iron Alloy (25-12 Class), for High-Temperature Service

    Available format(s):  Hardcopy, PDF

    Superseded date:  11-11-2014

    Language(s):  English

    Published date:  11-01-2007

    Publisher:  American Society for Testing and Materials

    Add to Watchlist

    Add To Cart

    Scope - (Show below) - (Hide below)

    1.1 This specification covers iron-base, heat-resisting alloy castings of the 25 % chromium, 12 % nickel class, intended for structural elements, containers, and supports in electric furnaces, petroleum still tube supports, and for similar applications up to 2000°F [1095°C]. The purchaser should inform the manufacturer when the service temperatures are to exceed 1800F [980C].

    1.2 In the absence of significant proportions of elements other than those prescribed in Section 4 , the two types of alloys covered by this specification may in general be distinguished as follows:

    1.2.1 Type I Alloys characterized by relatively low limiting creep stress at temperatures between 1500 and 2000°F [815 and 1095°C], and relatively high ductility at ordinary temperatures after aging for short periods at temperatures between 1300 and 1500°F [705 and 815°C].

    1.2.2 Type II Alloys having relatively high limiting creep stress but which may develop low ductility at ordinary temperatures when aged for short periods at temperatures between 1350 and 1500°F [730 and 815°C].

    1.3 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with the specification.

    General Product Information - (Show below) - (Hide below)

    Committee A 01
    Document Type Standard
    Publisher American Society for Testing and Materials
    Status Superseded
    Superseded By
    • Access your standards online with a subscription

      Features

      • Simple online access to standards, technical information and regulations
      • Critical updates of standards and customisable alerts and notifications
      • Multi - user online standards collection: secure, flexibile and cost effective