MIL-DTL-32477 Base Document:2013
|
ROD AND BAR, COBALT-NICKEL-CHROMIUM-IRON-MOLYBDENUM ALLOY, FOR USE IN CRITICAL SEAWATER APPLICATIONS |
SAE AS 7237 : 2012
|
RIVETS, NICKEL ALLOY, CORROSION AND HEAT RESISTANT 47.5NI-22CR-1.5CO-9.0MO-0.60W-18.5FE SOLUTION HEAT TREATED PROCUREMENT SPECIFICATION FOR |
SAE AMS 5960 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT SHEET, STRIP, AND FOIL, NI - 18CR - 2.8MO - 5.5CB(NB) - 0.70TI - 1.50AL - 10FE - 9CO - 1W, VACUUM INDUCTION MELTED AND CONSUMABLE ELECTRODE REMELTED, SOLUTION HEAT TREATED |
ASTM B 758 : 2000 : R2006
|
Standard Specification for Nickel-Chromium-Molybdenum-Tungsten Alloys (UNS N06110) Welded Tube |
SAE AMS 5843 : 2016
|
COBALT-NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS 19CR - 36CO - 25NI - 7.0MO - 0.50CB (NB) - 2.9TI - 0.20AL - 9.0FE VACUUM INDUCTION PLUS VACUUM CONSUMABLE ELECTRODE MELTED SOLUTION HEAT TREATED, WORK STRENGTHENED, AND AGED |
SAE MAM 5598 : 2000
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SHEET, STRIP, AND PLATE 72NI - 15.5CR - 0.95(CB + TA) - 2.5TI - 0.70AL - 7.0FE CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE |
SAE AMS 5536 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 47.5NI - 22CR - 1.5CO - 9.0MO - 0.60W - 18.5FE, SOLUTION HEAT TREATED |
SAE MAM 5914 : 2003
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SHEET, STRIP, AND FOIL 52.5NI - 19CR - 3.0MO - 5.0CB - 0.90TI - 0.50AL - 18FE CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED PRECISION COLD ROLLED, SOLUTION HEAT TREATED |
ASTM F 1377 : 2013 : REDLINE
|
Standard Specification for Cobalt-28Chromium-6Molybdenum Powder for Coating of Orthopedic Implants (UNS R30075) |
ASTM F 31 : 2016 : REDLINE
|
Standard Specification for Nickel-Chromium-Iron Sealing Alloys |
SAE AMS 5587 : 2016
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING, 47.5NI - 22CR - 1.5CO - 9.0MO - 0.60W - 18.5FE, SOLUTION HEAT TREATED |
SAE AMS 5663 : 2016
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS 52.5NI - 19CR - 3.0MO - 5.1CB (NB) - 0.90TI - 0.50AL - 18FE CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED 1775 DEGREES F (968 DEGREES C) SOLUTION AND PRECIPITATION HEAT TREATED |
SAE ARP 4926 : 2011
|
ALLOY VERIFICATION AND CHEMICAL COMPOSITION INSPECTION OF WELDING WIRE |
SAE AMS 5223 : 2012
|
IRON-NICKEL ALLOY, STRIP, 49Fe 5.3Cr 42Ni 2.5Ti 0.55Al, SOLUTION HEAT TREATED, COLD ROLLED, 10% REDUCTION |
ASTM B 757 : 2000
|
Standard Specification for Nickel-Chromium-Molybdenum-Tungsten-Alloys (UNS N06110) Welded Pipe |
SAE AMS 5704 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, FORGINGS 57NI - 19.5CR - 13.5CO - 4.3MO - 3.0TI - 1.4AL - 0.05ZR - 0.006B CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED 1825 TO 1900 DEGREES F (996 TO 1038 DEGREES C) SOLUTION, STABILIZATION, AND PRECIPITATION HEAT TREATED |
SAE AMS 5583 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SEAMLESS TUBING 72NI - 15.5CR - 0.95CB - 2.5TI - 0.70AL - 7.0FE, VACUUM MELTED, SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 170 KSI (1172 MPA) TENSILE STRENGTH |
SAE AMS 5961 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WIRE, 74NI - 15.5CR - 8.0FE, COLD REDUCED, SPRING TEMPER |
SAE AMS5530H:1988(S2017)
|
ALLOY SHEET, STRIP, AND PLATE, CORROSION AND HEAT RESISTANT, 58NI - 15.5CR - 16MO - 3.8W - 5.5FE, SOLUTION HEAT TREATED |
SAE AMS 5842 : 2016
|
COBALT-NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS 19CR - 36CO - 25NI - 7.0MO - 0.50CB (NB) - 2.9TI - 0.20AL - 9.0FE VACUUM INDUCTION PLUS VACUUM CONSUMABLE ELECTRODE MELTED SOLUTION HEAT TREATED AND WORK STRENGTHENED |
SAE AMS 5665 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, BARS, FORGINGS, AND RINGS, 74NI - 15.5CR - 8.0FE |
SAE AMS 5834 : 2014
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, ROUND WIRE 20CR - 15NI - 40CO - 7.0MO - 16FE VACUUM INDUCTION PLUS CONSUMABLE ELECTRODE MELTED SOLUTION HEAT TREATED, COLD DRAWN, AND AGED |
SAE AMS 5402 : 2004
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, INVESTMENT CASTINGS 62NI - 21.5CR - 9.0MO - 3.6CB (NB) AS CAST |
SAE AMS 5771 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 74NI - 7.0CR - 16.5 MO, SOLUTION HEAT TREATED |
SAE AMS 5786 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 62.5NI - 5.0CR - 24.5MO - 5.5FE |
SAE AMS 5589 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SEAMLESS TUBING 52.5NI - 19CR - 3.0MO - 5.1CB - 0.90TI - 0.50AL - 18FE CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED, 1775 DEGREES F (968 DEGREES C), SOLUTION HEAT TREATED |
SAE AMS 5397 : 2015
|
ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT-RESISTANT 50NI - 9.5CR - 15CO - 3.0MO - 4.8TI - 5.5AL - 0.015B - 0.95V - 0.06ZR VACUUM MELTED, VACUUM CAST, AS CAST |
SAE AMS 5706 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 57NI - 19.5CR - 13.5CO - 4.3MO - 3.0TI - 1.4AL - 0.006B - 0.05ZR, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 1825 TO 1900 DEGREES F SOLUTION HEAT TREATED |
SAE AMS 5888C : 2009(R2015)
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, PLATE, 54NI - 22CR - 12.5CO - 9.0MO - 1.2AL, ANNEALED |
SAE AMS 5715 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 60.5NI - 23CR - 14FE - 1.4AL, ANNEALED |
ASTM E 1473 : 2016 : REDLINE
|
Standard Test Methods for Chemical Analysis of Nickel, Cobalt and High-Temperature Alloys |
SAE AMS 5390 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, INVESTMENT CASTINGS, 47.5NI - 22CR - 1.5CO - 9MO - 0.60W - 18.5FE (N-12MV) AS-CAST |
ASTM C 983 : 1991
|
Test Methods for Chemical and Instrumental Analysis of Metallic Core Components in Liquid Metal Fast-Breeder Reactors (LMFBR) (Withdrawn 1996) |
ASTM F 468M:2006
|
Standard Specification for Nonferrous Bolts, Hex Cap Screws, and Studs for General Use [Metric] |
SAE AMS 5872 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 48NI - 20CR - 20CO - 5.9MO - 2.2TI - 0.45AL, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, SOLUTION HEAT TREATED |
ASTM F 3213 : 2017
|
Standard for Additive Manufacturing – Finished Part Properties – Standard Specification for Cobalt-28 Chromium-6 Molybdenum via Powder Bed Fusion |
ASTM F 90 : 2014 : REDLINE
|
Standard Specification for Wrought Cobalt-20Chromium-15Tungsten-10Nickel Alloy for Surgical Implant Applications (UNS R30605) |
ASTM F 1314 : 2018 : REDLINE
|
Standard Specification for Wrought Nitrogen Strengthened 22 Chromium–13 Nickel–5 Manganese–2.5 Molybdenum Stainless Steel Alloy Bar and Wire for Surgical Implants (UNS S20910) |
ASTM B 757 : 2000 : R2016
|
Standard Specification for Nickel-Chromium-Molybdenum-Tungsten-Alloys (UNS N06110) Welded Pipe (Withdrawn 2021) |
ASTM B 445 : 1987
|
Specification for Nickel-Chromium-Iron-Columbium-Molybdenum-Tungsten Alloy (UNS N06102) Seamless Pipe and Tube (Withdrawn 1995) |
ASTM B 519 : 1992
|
Specification for Nickel-Chromium-Iron-Columbium-Molybdenum-Tungsten Alloy (UNS N06102) Plate, Sheet, and Strip (Withdrawn 1995) |
ASTM B 688 : 1996
|
Standard Specification for Chromium-Nickel-Molybdenum-Iron (UNS N08366 and UNS N08367) Plate, Sheet, and Strip |
SAE AMS 5401 : 2004
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, INVESTMENT CASTINGS, 62NI - 21.5CR - 9.0MO - 3.6CB (NB), VACUUM MELTED, VACUUM CAST, AS CAST |
ASTM F 1466 : 1999 : R2015
|
Standard Specification for Iron-Nickel-Cobalt Alloys for Metal-to-Ceramic Sealing Applications |
ASTM F 1684 : 2006 : R2011
|
Standard Specification for Iron-Nickel and Iron-Nickel-Cobalt Alloys for Low Thermal Expansion Applications |
ASTM E 353 : 2014 : REDLINE
|
Standard Test Methods for Chemical Analysis of Stainless, Heat-Resisting, Maraging, and Other Similar Chromium-Nickel-Iron Alloys |
SAE AMS 5667 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS 72NI - 15.5CR - 0.95CB - 2.5TI - 0.70AL - 7.0FE EQUALIZED, PRECIPITATION HARDENABLE |
SAE AMS 5914 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SHEET, STRIP, AND FOIL 52.5NI - 19CR - 3.0MO - 5.0CB - 0.90TI - 0.50AL - 18FE, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED PRECISION COLD ROLLED, SOLUTION HEAT TREATED |
SAE AMS 5940 : 2014
|
ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS 34CO - 3.0CR - 28NI - 3.0CB(NB) - 5.5AL - 0.008B - 25.5FE MULTIPLE MELTED, HIGH TEMPERATURE, OXIDATION-RESISTANT, LOW EXPANSION SOLUTION HEAT TREATED, PRECIPITATION-HARDENABLE |
API 6A718 REDLINE : 2009
|
NICKEL BASE ALLOY 718 (UNS N07718) FOR OIL AND GAS DRILLING AND PRODUCTION EQUIPMENT |
SAE AMS 5874 : 2012
|
ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 29FE - 22CR - 21NI - 18.5CO - 3.2MO - 2.8W - 0.78TA - 0.30AL - 0.05ZR - 0.05LA - 0.20N SOLUTION HEAT TREATED |
ASTM B 758 : 2000 : R2016
|
Standard Specification for Nickel-Chromium-Molybdenum-Tungsten Alloys (UNS N06110) Welded Tube (Withdrawn 2021) |
SAE AMS 5871 : 2015
|
ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP AND PLATE, 21CR - 32.5NI - 0.38TI - 0.38AL - 45FE, SOLUTION HEAT TREATED |
API 6ACRA : 2015 : INC : ADD 1 : 2017
|
AGE-HARDENED NICKEL-BASED ALLOYS FOR OIL AND GAS DRILLING AND PRODUCTION EQUIPMENT |
ASTM B 688 : 1996 : R2014
|
Standard Specification for Chromium-Nickel-Molybdenum-Iron (UNS N08366 and UNS N08367) Plate, Sheet, and Strip |
SAE AMS 5711 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 65NI - 15.8CR - 15.2MO - 0.30AL - 0.05LA, SOLUTION HEAT TREATED |
SAE MAM 5599 : 2003
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SHEET, STRIP, AND PLATE 62NI - 21.5CR - 9.0MO - 3.7 (CB+TA) ANNEALED |
SAE AMS 5442 : 2017
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, NI - 18CR - 2.8MO - 5.5CB(NB) - 0.70TI - 1.50AL - 10FE - 9CO - 1W, CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED, 1775 DEGREES F (968 DEGREES C) SOLUTION AND PRECIPITATION HEAT TREATED |
BS ISO 12891-2:2014
|
Retrieval and analysis of surgical implants Analysis of retrieved surgical implants |
SAE AMS 5396 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, INVESTMENT CASTINGS, 65NI - 28MO - 5.5FE - 0.40V (N-12MV), AS-CAST |
SAE AMS 5873 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 65NI - 15.8CR - 15.2MO - 0.30AI - 0.05LA, CONSUMABLE ELECTRODE REMELTED, SOLUTION HEAT TREATED |
ASTM F 3042 : 2013
|
Standard Specification for Nonferrous Hex Socket, Slotted Headless, and Square Head Set Screws |
SAE AMS 5399 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, INVESTMENT CASTINGS, 52NI - 19CR - 11CO - 9.8MO - 3.2TI - 1.6AL - 0.006B, VACUUM-MELTED, VACUUM-CAST, SOLUTION HEAT TREATED |
ASTM F 2581 : 2012
|
Standard Specification for Wrought Nitrogen Strengthened 11Manganese-17Chromium-3Molybdenum Low-Nickel Stainless Steel Alloy Bar and Wire for Surgical Implants (UNS S29225) |
SAE AMS 5875 : 2012
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, STRIP, 20CR - 15NI - 40CO - 7.0MO - 16FE, SOLUTION HEAT TREATED, COLD ROLLED, AND AGED, VACUUM INDUCTION PLUS VACUUM CONSUMABLE ELECTRODE MELTED |
SAE AMS 5598 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 72NI - 15.5CR - 0.95 (CB (NB) + TA) - 2.5TI - 0.70AL - 7.0FE, CONSUMABLE ELECTRODE, REMELTED OR VACUUM INDUCTION MELTED, SOLUTION HEAT TREATED, PRECIPITATION-HARDENABLE |
SAE AMS 5383 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, INVESTMENT CASTINGS, 52.5NI - 19CR - 3.0MO - 5.1CB(NB) - 0.90TI - 0.60AL - 18FE, VACUUM MELTED HOMOGENIZATION AND SOLUTION HEAT TREATED |
SAE AMS 5750 : 2017
|
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT, NICKEL BASE - 15.5CR - 16MO - 3.8W - 5.5FE, SOLUTION HEAT TREATED |
SAE AMS 5846 : 2016
|
ALLOY, CORROSION AND HEAT-RESISTANT, BARS AND FORGINGS, 53NI - 15CR - 18.5CO - 5.0MO - 3.2TI - 4.2AL - 0.03B, DOUBLE VACUUM MELTED SOLUTION, STABILIZATION, AND PRECIPITATION HEAT TREATED |
SAE AMS 5919 : 2013
|
COBALT-NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, ROUND BARS 19CR - 36CO - 25NI - 7.0MO - 0.50CB (NB) - 2.9TI - 0.20AL - 9.0FE VACUUM INDUCTION PLUS VACUUM CONSUMABLE ELECTRODE MELTED SOLUTION HEAT TREATED AND WORK STRENGTHENED, MODIFIED STRENGTH |
SAE AMS 5532 : 2017
|
IRON ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 30FE - 21CR - 20NI - 20CO - 3.0MO - 2.5W - 1.0CB(NB) - 0.15N, SOLUTION HEAT TREATED |
ASTM F 2581 : 2012 : R2017
|
Standard Specification for Wrought Nitrogen Strengthened 11Manganese-17Chromium-3Molybdenum Low-Nickel Stainless Steel Alloy Bar and Wire for Surgical Implants (UNS S29225) |
SAE AMS 5373 : 2017
|
ALLOY CASTINGS, SAND, CORROSION AND HEAT RESISTANT, 16CO - 29CR - 4.5W, AS CAST, UNS R30006 |
SAE AMS 5841 : 2016
|
COBALT-NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS 19CR - 36CO - 25NI - 7.0MO - 0.50CB (NB) - 2.9TI - 0.20AL - 9.0FE VACUUM INDUCTION PLUS VACUUM CONSUMABLE ELECTRODE MELTED SOLUTION HEAT TREATED FOR WORK STRENGTHENING |
SAE AMS5802E : 2017
|
IRON-NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 41FE - 37.5NI - 14CO - 4.8CB (NB) - 1.5TI, VACUUM MELTED, LOW EXPANSION |
AWS A5.35/A5.35M : 2015
|
SPECIFICATION FOR COVERED ELECTRODES FOR UNDERWATER WET SHIELDED METAL ARC WELDING |
SAE AMS 7727F : 2017(S2019)
|
IRON-NICKEL-COBALT ALLOY, BARS AND FORGINGS, 53FE - 29NI - 17CO, LOW EXPANSION, GLASS SEALING |
SAE AMS 5666H : 2016
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, EXTRUSIONS, AND RINGS, 62NI - 21.5CR - 9.0MO - 3.65CB (NB), ANNEALED |
SAE AMS 5701 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 41.5NI - 16CR - 37FE - 2.9CB (NB) - 1.8TI, CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED, 1800 DEGREES F (982 DEGREES C) SOLUTION HEAT TREATED |
SAE AMS 5676 : 2011
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 80NI - 20CR |
ASTM B 688 : 1996 : R2004
|
Standard Specification for Chromium-Nickel-Molybdenum-Iron (UNS N08366 and UNS N08367) Plate, Sheet, and Strip |
SAE AMS 5768 : 2018
|
ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 21CR - 20NI - 20CO - 3.0MO - 2.5W - 1.0CB - 0.15N - 31FE, SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS 5870 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 60.5NI - 23CR - 14FE - 0.35TI - 1.4AL, SOLUTION HEAT TREATED |
SAE AMS 5376 : 2013
|
ALLOY, CORROSION AND HEAT RESISTANT, INVESTMENT CASTINGS, 30FE - 21CR - 20NI - 20CO - 3.0MO - 2.5W - 1.0CB - 0.15N, AS CAST |
SAE MAM 5536 : 2003
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SHEET, STRIP, AND PLATE 47.5NI - 22CR - 1.5CO 9.0MO - 0.60W - 18.5FE SOLUTION HEAT TREATED |
SAE AMS 5755 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 64NI - 5.0CR - 24.5MO - 5.5FE, SOLUTION HEAT TREATED |
ASTM F 3056 : 2014
|
Standard Specification for Additive Manufacturing Nickel Alloy (UNS N06625) with Powder Bed Fusion |
ASTM F 3056 : 2014 : EDT 1
|
Standard Specification for Additive Manufacturing Nickel Alloy (UNS N06625) with Powder Bed Fusion |
ASTM F 467M : 2006 : REV A : EDT 2
|
Standard Specification for Nonferrous Nuts for General Use (Metric) |
ASTM F 467M : 2006 : REV A : EDT 1
|
Standard Specification for Nonferrous Nuts for General Use [Metric] |
ASTM F 3055 : 2014
|
Standard Specification for Additive Manufacturing Nickel Alloy (UNS N07718) with Powder Bed Fusion |
ASTM F 3055 : 2014 : EDT 1
|
Standard Specification for Additive Manufacturing Nickel Alloy (UNS N07718) with Powder Bed Fusion |
ASTM F 561 : 2013
|
Standard Practice for Retrieval and Analysis of Medical Devices, and Associated Tissues and Fluids |
ASME PV CODE 2C : 2017
|
BOILER AND PRESSURE VESSEL CODE - MATERIALS - SPECIFICATIONS FOR WELDING RODS, ELECTRODES, AND FILLER METALS |
SAE AMS 5702 : 2018
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 41.5NI - 16CR - 37FE - 2.9CB (NB) - 1.8TI, CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED, 1750 DEGREES F (954 DEGREES C) SOLUTION HEAT TREATED |
SAE AMS 5441 : 2016
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, NI - 18CR - 2.8MO - 5.5CB(NB) - 0.70TI - 1.50AL - 10FE - 9CO - 1W, CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED, 1775 DEGREES F (968 DEGREES C) SOLUTION HEAT TREATED, PRECIPITATION-HARDENABLE |
ASTM B 804 : 2002 : R2007
|
Standard Specification for UNS N08367 and UNS N08926 Welded Pipe |
ASTM B 804 : 2002 : R2013
|
Standard Specification for UNS N08367 and UNS N08926 Welded Pipe |
SAE MAM 5401 : 2003
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, INVESTMENT CASTINGS 62NI - 21.5CR - 9.0MO - 3.6CB VACUUM MELTED, VACUUM CAST AS CAST |
SAE AMS 5747 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 72NI - 15.5CR - 0.95CB(NB) - 2.5TI - 0.70AL - 7.0FE, SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE |
SAE AMS 5916 : 2017
|
ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 35FE - 24CR - 37NI - 0.65CB(NB) - 0.2N, ANNEALED |
SAE AMS 5225 : 2014
|
IRON-NICKEL ALLOY, STRIP, 49FE - 5.3CR - 42NI - 2.5TI - 0.55AL, SOLUTION HEAT TREATED, COLD ROLLED, 50% REDUCTION |
SAE AMS 5389 : 1987(R2017)
|
ALLOY CASTINGS, SAND, CORROSION AND HEAT RESISTANT, 55NI - 16.5CR - 17MO - 4.5W - 5.8FE - 0.40V, SOLUTION HEAT TREATED |
SAE AMS 5889 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SHEET AND STRIP, 54NI - 22CR - 12.5CO - 9.0MO - 1.2AL, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, ANNEALED |
SAE AS 7232 : 2012
|
RIVETS, SOLID AND TUBULAR, NICKEL ALLOY CORROSION AND HEAT RESISTANT 74NI - 15.5CR - 8.0FE PROCUREMENT SPECIFICATION FOR |
SAE AMS 5709 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, BARS AND FORGINGS, 58NI - 19.5CR - 13.5CO - 4.3MO - 3.0TI - 1.4AL - 0.05ZR - 0.006B, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 1975 DEGREE F (1079 DEGREE C) SOLUTION, STABILIZATION, AND PRECIPITATION HEAT TREATED |
MIL-P-83348 Revision A:1983
|
POWDER, PLASMA SPRAY |
ASTM B 853 : 2016 : REDLINE
|
Standard Specification for Powder Metallurgy (PM) Boron Stainless Steel Structural Components |
MIL-P-85856 Base Document:1988
|
POWDER MATERIALS FOR FLAME AND PLASMA SPRAYED COATINGS GENERAL SPECIFICATION FOR |
API 6A718 RUSSIAN : 2009
|
NICKEL BASE ALLOY 718 (UNS N07718) FOR OIL AND GAS DRILLING AND PRODUCTION EQUIPMENT |
SAE AMS5766E:2014
|
ALLOY, CORROSION AND HEAT-RESISTANT, BARS AND FORGINGS, 21CR - 32.5NI - 0.38TI - 0.38AL - 45FE, SOLUTION HEAT TREATED |
SAE AMS 5797E : 2002(S2018)
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, COVERED WELDING ELECTRODES, 51.5CO - 20CR - 10NI - 15W |
SAE AS 7246 : 2012
|
INSERTS, SCREW THREADS, HELICAL COIL 72NI-15.5CR-0.95(CB+TA)-2.5TI-0.70AL-7.0FE CORROSION AND HEAT RESISTANT ALLOY PROCUREMENT SPECIFICATION FOR |
SAE AMS 5892 : 2014
|
ALLOY, SHEET AND STRIP, 42FE - 37.5NI - 14CO - 4.8CB (NB) - 1.6TI, SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE, MULTIPLE MELTED, HIGH TEMPERATURE, LOW EXPANSION |
SAE AMS 5845 : 2014
|
ALLOY, CORROSION-RESISTANT, ROUND BARS 20CR - 35NI - 35CO - 10MO VACUUM INDUCTION PLUS CONSUMABLE ELECTRODE VACUUM REMELTED SOLUTION HEAT TREATED, WORK STRENGTHENED, AND AGED |
SAE AMS5751F : 1982(S2017)
|
Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant 54Ni - 17.5Cr - 16.5Co - 4.0Mo - 2.9Ti - 2.9Al - 0.006B Solution, Stabilization, and Precipitation Heat Treated Consumable Electrode or Vacuum Induction Melted
|
ASTM F 2281 : 2004 : R2012
|
Standard Specification for Stainless Steel and Nickel Alloy Bolts, Hex Cap Screws, and Studs, for Heat Resistance and High Temperature Applications |
SAE AMS 5713K : 2016
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 53NI - 19CR - 11CO - 9.8MO - 3.2TI - 1.6AL - 0.006B, VACUUM MELTED, SOLUTION AND PRECIPITATION HEAT TREATED |
ASTM F 468M : 2006 : R2012
|
Standard Specification for Nonferrous Bolts, Hex Cap Screws, and Studs for General Use (Metric) |
SAE AMS 5886 : 2014
|
ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS 50NI - 20CR - 20CO - 5.8MO - 2.2TI - 0.45AL CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED 2100 DEGREES F (1149 DEGREES C) SOLUTION HEAT TREATED |
SAE AMS 5772 E: 2016
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 40CO - 22CR - 22NI - 14.5W - 0.07LA, SOLUTION HEAT TREATED |
SAE AMS 5854 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, WIRE, FORGINGS, AND RINGS, 61NI - 20.5CR - 8.5MO - 3.4CB(NB) - 1.3TI - 5.0FE, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED SOLUTION HEAT TREATED |
SAE AMS 5800 : 2006
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 54NI - 19CR - 11CO - 10MO - 3.2TI - 1.5AL - 0.006B, VACUUM INDUCTION MELTED |
SAE AMS 4778 : 2013
|
NICKEL ALLOY, BRAZING FILLER METAL, 92NI - 4.5SI - 3.1B, 1800 TO 1900 DEGREES F SOLIDUS-LIQUIDUS RANGE |
SAE AMS 5661 : 2012
|
NICKEL-IRON ALLOY, CORROSION AND HEAT RESISTANT, BARS, FORGINGS, AND RINGS - 42.5NI - 12.5CR - 5.8MO - 2.9TI - 0.015B - 35FE - CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED SOLUTION, STABILIZATION, AND PRECIPITATION HEAT TREATED |
SAE AMS 5962 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, ROUND BARS AND WIRE, 52.5NI - 19CR - 3.0MO - 5.1CB - 0.90TI - 0.50AL - 18FE, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 1775 DEGREES F (968 DEGREES C) SOLUTION TREATED AND WORK STRENGTHENED, PRECIPITATION HARDENABLE |
ASTM F 139 : 2012
|
Standard Specification for Wrought 18Chromium-14Nickel-2.5Molybdenum Stainless Steel Sheet and Strip for Surgical Implants (UNS S31673) |
ASTM F 2281 : 2004
|
Standard Specification for Stainless Steel and Nickel Alloy Bolts, Hex Cap Screws, and Studs, for Heat Resistance and High Temperature Applications |
SAE AMS 5586 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WELDED TUBING, 57NI - 19.5CR - 13.5CO - 4.2MO - 2.9TI - 1.4AL - 0.006B - 0.08ZR, CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED, ANNEALED |
API 6ACRA : 2015 : ERR 1 : 2015
|
AGE-HARDENED NICKEL-BASED ALLOYS FOR OIL AND GAS DRILLING AND PRODUCTION EQUIPMENT |
SAE AMS 5890 : 2015
|
NICKEL, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND EXTRUSIONS, THORIA DISPERSION STRENGTHENED, 2.2THO[2], STRESS-RELIEVED |
SAE AMS 5555 : 2013
|
NICKEL WIRE AND RIBBON 99NI |
SAE AMS 5385 : 2013
|
COBALT ALLOY, CORROSION AND HEAT RESISTANT, INVESTMENT CASTINGS, 62MO - 27CR - 2.8NI - 5.5MO, AS-CAST |
SAE AMS 5541 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SHEET AND STRIP 73NI - 15.5CR - 2.4TI - 0.7AL - 7.0FE ANNEALED |
SAE AMS 5844 : 2014
|
ALLOY, CORROSION-RESISTANT, ROUND BARS, 20CR - 35NI - 35CO - 10MO, VACUUM INDUCTION PLUS CONSUMABLE ELECTRODE VACUUM REMELTED, SOLUTION HEAT TREATED AND WORK STRENGTHENED |
AWS A5.34/A5.34M : 2013
|
SPECIFICATION FOR NICKEL-ALLOY ELECTRODES FOR FLUX CORED ARC WELDING |
SAE AMS 5410 : 2017
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, INVESTMENT CASTINGS, 61NI - 16CR - 8.5CO - 1.8MO - 2.6W - 0.85CB (NB) - 3.4TI - 1.8TA - 3.4AL - 0.010B - 0.05ZR, VACUUM MELTED, VACUUM CAST AS CAST, OR SOLUTION TREATED, OR SOLUTION AND PRECIPITATION HARDENED |
SAE AMS 7000 : 2018
|
LASER-POWDER BED FUSION (L-PBF) PRODUCED PARTS, NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, 62NI - 21.5CR - 9.0MO - 3.65NB STRESS RELIEVED, HOT ISOSTATIC PRESSED AND SOLUTION ANNEALED |
ASTM B 757 : 2000 : R2006
|
Standard Specification for Nickel-Chromium-Molybdenum-Tungsten-Alloys (UNS N06110) Welded Pipe |
SAE AMS 5878 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 59NI - 22CR - 2MO - 14W - 0.35AI - 0.03LA, SOLUTION HEAT TREATED |
SAE MAM 4778 : 2003
|
NICKEL ALLOY, BRAZING FILLER METAL, 92NI - 4.5SI - 3.1B, 980 TO 1040 DEGREE C SOLIDUS-LIQUIDUS RANGE |
ASTM F 467M : 2006 : REV A : R2012
|
Standard Specification for Nonferrous Nuts for General Use (Metric) |
ASTM A 781/A781M : 2018-02
|
SPECIFICATION FOR CASTINGS, STEEL AND ALLOY, COMMON REQUIREMENTS, FOR GENERAL INDUSTRIAL USE |
ASTM F 1684 : 2006 : R2016
|
Standard Specification for Iron-Nickel and Iron-Nickel-Cobalt Alloys for Low Thermal Expansion Applications |
ASTM E 350 : 2012-09
|
TEST METHODS FOR CHEMICAL ANALYSIS OF CARBON STEEL, LOW-ALLOY STEEL, SILICON ELECTRICAL STEEL, INGOT IRON, AND WROUGHT IRON |
SAE AMS 5682 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 78NI - 20CR |
SAE AMS 5830 : 2012
|
NICKEL-IRON ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 12.5CR - 42.5NI - 6.0MO - 2.7TI - 0.015B - 35FE |
SAE AMS 5887 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 54NI - 22CR - 12.5CO - 9.0MO - 1.2AL, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, ANNEALED |
SAE AMS 5668 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 72NI - 15.5CR - 7.0FE - 2.5TI - 1.0CB (NB) - 0.70AL, 2100 DEGREES F (1149 DEGREES C) SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS 5835 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 72NI - 3.2MN - 20CR - 2.5CB - 0.48TI, VACUUM INDUCTION MELTED, ENVIRONMENT CONTROLLED PACKAGING |
SAE AMS 5683:2012(S2017)
|
ALLOY WELDING WIRE, CORROSION AND HEAT RESISTANT, 75NI - 15.5CR - 8.0FE |
SAE AMS 5384 : 2017
|
ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT RESISTANT, 53NI - 18CR - 18CO - 4.0MO - 2.9TI - 2.9AL - 0.006B, VACUUM-MELTED, VACUUM-CAST, SOLUTION AND PRECIPITATION HEAT TREATED |
SAE AMS 5544 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 57NI - 19.5CR - 13.5CO - 4.2MO - 3.0TI - 1.4AL - 0.05ZR - 0.006B, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, ANNEALED |
ASTM B 758 : 2000 : R2011
|
Standard Specification for Nickel-Chromium-Molybdenum-Tungsten Alloys (UNS N06110) Welded Tube |
ASTM B 758 : 2000
|
Standard Specification for Nickel-Chromium-Molybdenum-Tungsten Alloys (UNS N06110) Welded Tube |
SAE AMS 5596 : 2017
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, FOIL AND PLATE, 52.5NI - 19CR - 3.0MO - 5.1CB (NB) - 0.90TI - 0.50AL - 18FE, CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED, 1775 DEGREES F (968 DEGREES C) SOLUTION HEAT TREATED |
SAE AMS 5597 : 2016
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SHEET, STRIP, AND PLATE, 52.5NI - 19CR - 3.0MO - 5.1CB (NB) - 0.90TI - 0.50AL - 18FE, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 1950 DEGREES F (1066 DEGREES C) SOLUTION HEAT TREATED |
SAE AMS 5915 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS AND FORGINGS, 57NI - 20CR - 10CO - 8.5MO - 2.1TI - 1.5AL - 0.005B, VACUUM INDUCTION AND CONSUMABLE ELECTRODE MELTED, SOLUTION HEAT TREATED, PRECIPITATION HEAT TREATABLE |
SAE AMS 5671 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 72NI - 15.5CR - 0.95CB - 2.5TI - 0.70AL - 7.0FE, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 1800 DEGREES F (982 DEGREES C) SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE |
SAE AMS 5832 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, WELDING WIRE, 52.5NI - 19CR - 3.0MO - 5.1CB(NB) - 0.90TI - 0.50AL - 18FE, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED |
ASTM B 518 : 1987
|
Specification for Nickel-Chromium-Iron-Columbium-Molybdenum-Tungsten Alloy (UNS N06102) Rod and Bar (Withdrawn 1995) |
API 6A718 : 2009
|
NICKEL BASE ALLOY 718 (UNS N07718) FOR OIL AND GAS DRILLING AND PRODUCTION EQUIPMENT |
ASTM F 2886 : 2017 : REDLINE
|
Standard Specification for Metal Injection Molded Cobalt-28Chromium-6Molybdenum Components for Surgical Implant Applications |
MIL-C-24689 Revision B:1992
|
COBALT ALLOY CASTINGS, WEAR AND CORROSION RESISTANT |
SAE AMS 5664 : 2017
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, BARS, FORGINGS, AND RINGS, 52.5NI - 19CR - 3.0MO - 5.1CB (NB) - 0.90TI - 0.50AL - 18FE, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED 1950 DEGREES F (1066 DEGREES C) SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE |
SAE AMS 5951 : 2017
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 57NI - 20CR - 10CO - 8.5MO - 2.1TI - 1.5AL - 0.005B, VACUUM INDUCTION AND CONSUMABLE ELECTRODE MELTED, SOLUTION HEAT TREATED, PRECIPITATION HEAT TREATABLE |
13/30242622 DC : 0
|
BS ISO 12891-2 - RETRIEVAL AND ANALYSIS OF SURGICAL IMPLANTS - PART 2: ANALYSIS OF RETRIEVED SURGICAL IMPLANTS |
ASTM B 757 : 2000 : R2011
|
Standard Specification for Nickel-Chromium-Molybdenum-Tungsten-Alloys (UNS N06110) Welded Pipe |
SAE AMS 5708 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, WIRE FORGINGS, AND RINGS, 58NI - 19.5CR - 13.5CO - 4.3MO - 3.0TI - 1.4AL - 0.05ZR - 0.006B, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 1975 DEGREES F (1079 DEGREES C) SOLUTION HEAT TREATED |
DOD C 24689 : A
|
COBALT ALLOY CASTINGS, WEAR AND CORROSION RESISTANT |
SAE AMS 5796 : 2012
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 52CO - 20CR - 10NI - 15W |
MIL-E-21562 Revision E:1989
|
ELECTRODES AND RODS - WELDING, BARE, NICKEL ALLOY |
SAE AMS 5884 : 2016
|
IRON-NICKEL ALLOY, BARS, FORGINGS, AND RINGS, 42FE - 37.5NI - 14CO - 4.8CB(NB) - 1.6TI, SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE MULTIPLE MELTED, HIGH TEMPERATURE, LOW EXPANSION |
ASTM F 562 : 2013 : REDLINE
|
Standard Specification for Wrought 35Cobalt-35Nickel-20Chromium-10Molybdenum Alloy for Surgical Implant Applications (UNS R30035) |
SAE AMS 5607 E: 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 73NI - 7.0CR - 16.5MO, SOLUTION HEAT TREATED |
SAE AMS 5964 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE NI - 18CR - 2.8MO - 5.5CB(NB) - 0.70TI - 1.50AL - 10FE - 9CO - 1W CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED |
SAE AMS 5608 : 2016
|
COBALT ALLOY, CORROSION AND HEAT RESISTANT, SHEET, STRIP, AND PLATE, 40CO - 22CR - 22NI - 14.5W - 0.07LA, SOLUTION HEAT TREATED |
SAE AMS 5391 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, INVESTMENT CASTINGS, 73NI - 0.14C - 13CR - 4.5MO - 2.3CB (NB) - 0.75TI - 6.0AL - 0.010B - 0.10ZR VACUUM CAST, AS-CAST |
SAE AMS 5377 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, INVESTMENT CASTINGS 73NI - 12CR - 4.5MO - 2.0CB - 0.70TI - 0.05C - 6.0AL - 0.010 - 0.10ZR VACUUM CAST, AS-CAST |
SAE AMS 5759M : 2015
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGING STOCK, FORGINGS, AND RINGS 52CO - 20CR - 10NI - 15W |
SAE AMS 5687N : 2018
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WIRE, 74NI - 15.5CR - 8.0FE, ANNEALED |
SAE AMS 5703 : 2018
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 41.5NI - 16CR - 37FE - 2.9CB - 1.8TI, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 1750 DEGREES F (954 DEGREES C) SOLUTION, STABILIZATION, AND PRECIPITATION HEAT TREATED |
SAE AMS 5662 : 2016
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS 52.5NI - 19CR - 3.0MO - 5.1CB (NB) - 0.90TI - 0.50AI - 18FE CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED 1775 DEGREES F (968 DEGREES C) SOLUTION HEAT TREATED, PRECIPITATION-HARDENABLE |
SAE AMS 5869 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE 62NI - 21.5CR - 9.0MO - 3.7CB SOLUTION HEAT TREATED |
SAE AMS 5540 : 2017
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 74NI - 15.5CR - 8.0FE, ANNEALED |
SAE AMS 5789 : 2014
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE 54CO - 25.5CR - 10.5NI - 7.5W |
ASTM B 720 : 1993
|
Specification for Seamless UNS N08310 Tube (Withdrawn 1999) |
SAE AMS 5917 : 2011
|
METAL INJECTION MOLDED NICKEL BASED, ALLOY 718 PARTS, HOT ISOSTATICALLY PRESSED, SOLUTIONED AND AGED |
SAE AMS 5814 : 2011
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 52CO - 20CR - 20NI - 7.5TA, VACUUM MELTED |
SAE AMS 5829 : 2011
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 56NI - 19.5CR - 16.5CO - 2.5TI - 1.5AL, VACUUM INDUCTION MELTED |
SAE AMS 2280 : 2012
|
TRACE ELEMENT CONTROL, NICKEL ALLOY CASTINGS |
ASTM F 2229 : 2012 : REDLINE
|
Standard Specification for Wrought, Nitrogen Strengthened 23Manganese-21Chromium-1Molybdenum Low-Nickel Stainless Steel Alloy Bar and Wire for Surgical Implants (UNS S29108) |
SAE AMS 5707 : 2017
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS 57NI - 19.5CR - 13.5CO - 4.3MO - 3.0TI - 1.4AL - 0.05ZR - 0.006B CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED 1825 TO 1900 DEGREES F (996 TO 1038 DEGREES C) SOLUTION, STABILIZATION, AND PRECIPITATION HEAT TREATED |
SAE AMS 5833 : 2014
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, ROUND WIRE 20CR - 15NI - 40CO - 7.0MO - 16FE SOLUTION HEAT TREATED AND COLD DRAWN |
SAE AMS 5852 : 2001
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, BILLETS AND PREFORMS 55NI 15CR 17CO 5.0MO 3.5TI 4.0AI 0.025B, POWDER METALLURGY PRODUCT, HOT ISOSTATICALLY PRESSED |
SAE AMS 5550F :1988(S2017)
|
ALLOY SHEET, STRIP, AND PLATE, CORROSION AND HEAT RESISTANT, 80NI - 15.5CR - 0.62TI - 3.25AL, ANNEALED |
SAE AMS 5542 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 72NI - 15.5CR - 0.95CB(NB) - 2.5TI - 0.70AL - 7.0FE, ANNEALED |
SAE ARP 1313 : 2014
|
DETERMINATION OF TRACE ELEMENTS IN HIGH TEMPERATURE ALLOYS |
ASTM F 468M : 2006 : EDT 1
|
Standard Specification for Nonferrous Bolts, Hex Cap Screws, and Studs for General Use [Metric] |
SAE AMS 5894 : 2016
|
COBALT ALLOYS, BARS, SHEET, AND PLATE, 60CO - 28CR - 4.5W - 1.15C, SOLUTION HEAT TREATED |
SAE AMS 5670 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, BARS, FORGINGS, AND RINGS - 72NI - 15.5CR - 0.95CB - 2.5TI - 0.70AL - 7.0FE, 1800 DEGREE F (982 DEGREE C) SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE |
SAE AMS 5828 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, WELDING WIRE 57NI - 19.5CR - 13.5CO - 4.2MO - 3.1TI - 1.4AL - 0.006B, VACUUM INDUCTION MELTED, SOLUTION HEAT TREATED |
SAE AMS 5754 : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 47.5NI - 22CR - 1.5CO - 9.0MO - 0.60W - 18.5FE, SOLUTION HEAT TREATED |
ASTM F 1466 : 1999 : R2005
|
Standard Specification for Iron-Nickel-Cobalt Alloys for Metal-to-Ceramic Sealing Applications |
ASTM F 3160 : 2016
|
Standard Guide for Metallurgical Characterization of Absorbable Metallic Materials for Medical Implants |
ASTM E 38 : 1985
|
Methods for Chemical Analysis of Nickel-Chromium and Nickel-Chromium-Iron Alloys (Withdrawn 1989) |
ISO 12891-2:2014
|
Retrieval and analysis of surgical implants Part 2: Analysis of retrieved surgical implants |
SAE AMS 5879 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND FOIL, 62NI - 21.5CR - 9.0MO - 3.7CB (NB), COLD ROLLED AND ANNEALED |
SAE AMS 7726 H : 2000(S2017)
|
IRON-NICKEL-COBALT ALLOY, WIRE, 53FE - 2.9NI - 17CO, LOW EXPANSION, GLASS SEALING, ANNEALED |
SAE AMS 5837G : 2012
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 62NI - 21.5CR - 9.0MO - 3.7CB(NB) |
ASTM F 1058 : 2016 : REDLINE
|
Standard Specification for Wrought 40Cobalt-20Chromium-16Iron-15Nickel-7Molybdenum Alloy Wire, Strip, and Strip Bar for Surgical Implant Applications (UNS R30003 and UNS R30008) |
SAE AMS 7875 : 2017
|
POWDER, CHROMIUM CARBIDE PLUS NICKEL-CHROMIUM ALLOY, 75CR[2]C[3] + 25 (80NI - 20CR ALLOY) |
SAE AMS 5794 : 2002(R2013)
|
IRON ALLOY, CORROSION AND HEAT-RESISTANT, WELDING WIRE, 31FE - 21CR - 20NI - 20CO - 3.0MO - 2.5W - 1.0CB - 0.15N, ANNEALED |
SAE MAM 5706 : 2003
|
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT RESISTANT, 57NI - 19.5CR - 13.5CO - 4.3MO - 3.0TI - 1.4A1 - 0.006B - 0.05ZR, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 995 DEGREES - 1040 DEGREES C SOLUTION HEAT TREATED |
SAE AMS 5582 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SEAMLESS TUBING, 72NI - 15.5CR - 0.95CB - 2.5TI - 0.70AL - 7.0FE, SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE TO 155 KSI (1069 MPA) TENSILE STRENGTH |
SAE AMS 5593 : 2016
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, SHEET, STRIP, AND PLATE, 45.5NI - 25.5CR - 3.2CO - 3.2MO - 3.2W - 18.5FE, SOLUTION HEAT TREATED |
SAE AMS 5380 : 2013
|
COBALT ALLOY, CORROSION AND HEAT RESISTANT, INVESTMENT CASTINGS, 50.5CO - 26CR - 15NI - 6.0MO, AS-CAST |
SAE AMS 4780 : 2012
|
MANGANESE ALLOY, BRAZING FILLER METAL 66MN - 16NI - 16CO - 0.80B, 1770 TO 1875 F (966 TO 1024 C) SOLIDUS-LIQUIDUS RANGE |
SAE AMS 5375 : 1982
|
ALLOY CASTINGS, INVESTMENT, CORROSION AND HEAT RESISTANT 65.5CO - 25CR - 1.8NI - 5.0W AS CAST |
ASTM E 32 : 2015
|
Standard Practices for Sampling Ferroalloys and Steel Additives for Determination of Chemical Composition |
ASTM F 2281 : 2004 : R2017
|
Standard Specification for Stainless Steel and Nickel Alloy Bolts, Hex Cap Screws, and Studs, for Heat Resistance and High Temperature Applications |
SAE AMS 5966 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT RESISTANT, WELDING WIRE, 50NI - 20CR - 20CO - 5.9MO - 2.2TI - 0.45AI, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED |
SAE AMS 5660 : 2015
|
NICKEL-IRON ALLOY, CORROSION AND HEAT-RESISTANT, BARS AND FORGINGS, 12.5CR - 42.5NI - 6.0MO - 2.7TI - 0.015B - 34FE, CONSUMABLE ELECTRODE REMELTED OR VACUUM INDUCTION MELTED SOLUTION, STABILIZATION, AND PRECIPITATION HEAT TREATED |
SAE AMS 5699 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WIRE, 72NI - 15.5CR - 0.95CB - 2.5TI - 0.70AL - 7.0FE, SPRING TEMPER, PRECIPITATION HARDENABLE |
SAE AMS 5891 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 60NI - 22CR - 2.0MO - 14W - 0.35AL - 0.03LA, ANNEALED |
ASTM F 961 : 2014 : REDLINE
|
Standard Specification for 35Cobalt-35Nickel-20Chromium-10Molybdenum Alloy Forgings for Surgical Implants (UNS R30035) |
SAE AMS 5758 : 2014
|
ALLOY, CORROSION-RESISTANT, BARS, 20CR - 35NI - 35CO - 10MO, VACUUM INDUCTION PLUS CONSUMABLE ELECTRODE VACUUM REMELTED, SOLUTION HEAT TREATED FOR WORK STRENGTHENING |
SAE AMS 5537 : 2017
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, FOIL, AND PLATE, 52CO - 20CR - 10NI - 15W, SOLUTION HEAT TREATED |
SAE AMS 5580 : 2015
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SEAMLESS TUBING 74NI - 15.5CR - 8.0FE, ANNEALED |
ASTM B 804 : 2002 : R2018
|
Standard Specification for UNS N08367 and UNS N08926 Welded Pipe |
API STD 6ACRA:2015
|
AGE-HARDENED NICKEL-BASED ALLOYS FOR OIL AND GAS DRILLING AND PRODUCTION EQUIPMENT |
ASTM E 30 : 1989
|
Test Methods for Chemical Analysis of Steel, Cast Iron, Open-Hearth Iron, and Wrought Iron (Withdrawn 1995) |
SAE AMS 5606 : 2013
|
ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE 41.5NI - 16CR - 37FE - 2.9CB (NB) - 1.8TI CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED 1750 DEGREES F (954 DEGREES C) SOLUTION HEAT TREATED |
SAE AMS 5599 : 2016
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 62NI - 21.5CR - 9.0MO - 3.7 CB (NB), ANNEALED |
SAE AMS 5712 : 2016
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS, 53NI - 19CR - 11CO - 9.8MO - 3.2TI - 1.6AL - 0.006B, VACUUM MELTED, SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE |
ASTM F 1466 : 1999
|
Standard Specification for Iron-Nickel-Cobalt Alloys for Metal-to-Ceramic Sealing Applications |
SAE AMS 5795G : 1993(S2017)
|
IRON ALLOY, CORROSION AND HEAT RESISTANT, COVERED, WELDING ELECTRODES, 31FE - 21CR - 20NI - 20CO - 3.0MO - 2.5W - 1.0(CB + TA) |
SAE AMS 5788 F: 2012
|
COBALT ALLOY, CORROSION AND HEAT-RESISTANT, HARD FACING RODS AND WIRE, 62CO - 29CR - 4.5W - 1.2C |
SAE AMS 5698 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, WIRE, 72NI - 15.5CR - 0.95CB - 2.5TI - 0.70AL - 7.0FE, NO. 1 TEMPER, PRECIPITATION HARDENABLE |
SAE AMS 5605 : 2013
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET, STRIP, AND PLATE, 41.5NI - 16CR - 37FE - 2.9CB(NB) - 1.8TI, CONSUMABLE ELECTRODE OR VACUUM INDUCTION MELTED, 1800 DEGREES F (982 DEGREES C) SOLUTION HEAT TREATED |
SAE AMS 5388 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, INVESTMENT CASTINGS 53.3NI - 16.5CR - 17MO - 4.5W - 5.8FE - 0.40V (CW-12MW), AS-CAST |
SAE AMS7728J : 2000(2017)
|
IRON-NICKEL-COBALT ALLOY, SHEET, STRIP, AND PLATE, 53FE - 29NI - 17CO, LOW EXPANSION GLASS SEALING, ANNEALED |
SAE AMS 5791 : 2015
|
COBALT ALLOY, POWDER, PLASMA SPRAY, 56.5CO - 25.5CR - 10.5NI - 7.5W |
ASTM F 1684 : 2006
|
Standard Specification for Iron-Nickel and Iron-Nickel-Cobalt Alloys for Low Thermal Expansion Applications |
AWS C2.25/C2.25M : 2012
|
SPECIFICATION FOR THERMAL SPRAY FEEDSTOCK - WIRE AND RODS |
SAE AMS 5950 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, SHEET AND STRIP 52.5NI - 19CR - 3.0MO - 5.0CB - 0.90TI - 0.50AL - 18FE VACUUM INDUCTION AND CONSUMABLE ELECTRODE MELTED SOLUTION HEAT TREATED, PRECIPITATION HARDENABLE |
SAE AMS 5717 : 2014
|
NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, BARS, FORGINGS, AND RINGS 45.5NI - 25.5CR - 3.2CO - 3.2MO - 3.2W - 18.5FE SOLUTION HEAT TREATED |
SAE AMS 5918 : 2011
|
COBALT ALLOY, CORROSION AND HEAT RESISTANT, BARS, 62CO - 28CR - 6MO, WARM-WORKED |
SAE AMS 5387 : 2015
|
ALLOY, CORROSION AND HEAT RESISTANT, INVESTMENT CASTINGS, 60CO - 29CR - 4.5W, AS CAST |
SAE AMS 7510C:2006(S2017)
|
MAGNETS, RARE-EARTH/COBALT, PERMANENT, POWDER-METALLURGY PRODUCT |
SAE AMS 5714 : 2018
|
ALLOY BARS, FORGINGS, AND RINGS, CORROSION AND HEAT-RESISTANT, 73NI - 15.5CR - 2.5TI - 0.70AL - 7.0FE, PRECIPITATION-HARDENABLE |
SAE AMS 5920 : 2013
|
COBALT-NICKEL ALLOY, CORROSION AND HEAT-RESISTANT, ROUND BARS 19CR - 36CO - 25NI - 7.0MO - 0.50CB (NB) - 2.9TI - 0.20AL - 9.0FE VACUUM INDUCTION PLUS VACUUM CONSUMABLE ELECTRODE MELTED SOLUTION HEAT TREATED, WORK STRENGTHENED AND AGED, MODIFIED STRENGTH |
ASTM F 1466 : 1999 : R2010
|
Standard Specification for Iron-Nickel-Cobalt Alloys for Metal-to-Ceramic Sealing Applications |
ASTM F 563 : 2000
|
Standard Specification for Wrought Cobalt-20Nickel-20Chromium-3.5Molybdenum-3.5Tungsten-5Iron Alloy for Surgical Implant Applications (UNS R30563) (Withdrawn 2005) |
ASTM B 688 : 1996 : R2009
|
Standard Specification for Chromium-Nickel-Molybdenum-Iron (UNS N08366 and UNS N08367) Plate, Sheet, and Strip |
ASTM F 1537 : 2011 : REDLINE
|
Standard Specification for Wrought Cobalt-28Chromium-6Molybdenum Alloys for Surgical Implants (UNS R31537, UNS R31538, and UNS R31539) |
ASTM B 804 : 2002
|
Standard Specification for UNS N08367 and UNS N08926 Welded Pipe |