ELECTRO-DEPOSITION OF SILVER

Superseded date

30-04-2007

Published date

12-01-2013

CONTENTS
Preface
Section One - General
1 Scope
2 WARNING
3 Related Documents
4 Definitions
5 Information to be Supplied to the Processor
6 Process Control
Section Two - Process Requirements
7 General
8 Undercoats
9 Silver Plating
10 Washing
11 Heat Treatment
12 Heat Treatment of Aluminium Alloys
Section Three - Inspection and Test
13 Inspection
14 Selection of Test Samples
15 Visual Inspection
16 Adhesion
17 Thickness of Coating
18 Solderability
Annex A - Adhesion Tests
Annex B - Method for the Determination of Average Thickness

Contains requirements for the electro-deposition of silver on ferrous-base materials, copper-base materials, aluminium base materials, zinc base materials and nickel-base materials.

DevelopmentNote
Supersedes DEFSTAN 03-9/1(1975) & DTD 919B (07/2003)
DocumentType
Standard
PublisherName
UK Ministry of Defence Standards
Status
Superseded
SupersededBy
Supersedes

DEFSTAN 03-4/5(2006) : 2006 THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA
DEFSTAN 03-29/3(2002) : 2002 PROTECTION OF METALLIC SPRINGS AGAINST CORROSION
DEFSTAN 59-71(PT1)/2(1993) : 1993 CRIMPED ELECTRICAL CONNECTORS FOR COPPER CONDUCTORS - PART 1: GENERAL REQUIREMENTS
DEFSTAN 03-29/2(1997) : 1997 PROTECTION OF METALLIC SPRINGS AGAINST CORROSION
DEFSTAN 03-4/4(1998) : 1998 THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA
DEFSTAN 03-29/1(1988) : 1988 PROTECTION OF METALLIC SPRINGS AGAINST CORROSION

DEFSTAN 03-4/4(1998) : 1998 THE PRE-TREATMENT AND PROTECTION OF STEEL ITEMS OF SPECIFIED MAXIMUM TENSILE STRENGTH EXCEEDING 1450 MPA
DEFSTAN 03-2/3(1995) : 1995 CLEANING AND PREPARATION OF METAL SURFACES
BS 2011-2.1T:1981 Environmental testing. Tests Test T. Soldering

View more information
Sorry this product is not available in your region.

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.