Chemical Check Analysis Limits Nickel, Nickel Alloys, and Cobalt Alloys

Available format(s)

Hardcopy , PDF

Language(s)

English

Published date

14-09-2022

This specification defines limits of variation for determining acceptability of the composition of cast or wrought nickel, nickel alloy, and cobalt alloy parts and material acquired from a producer.

Committee
AMS F
DocumentType
Revision
Pages
7
PublisherName
SAE International
Status
Current
Supersedes

SAE AMS5893D:2023 Iron-Nickel Alloy, Bars, Forgings, and Rings and Stock for Rings, Forgings, and Heading 42Fe - 37.5Ni - 14Co - 4.8 (Cb + Ta)(Nb + Ta) - 1.6Ti Solution Heat Treated, Short-Time Precipitation Hardenable Multiple Melted, High Temperature, Low Expansion
SAE AMS5537K:2023 Cobalt Alloy, Corrosion- and Heat-Resistant, Sheet, Strip, Foil, and Plate 52Co - 20Cr - 10Ni - 15W Solution Heat Treated
SAE AMS5796F:2018(R2023) Cobalt Alloy, Corrosion- and Heat-Resistant, Welding Wire 52Co - 20Cr - 10Ni -15W
SAE AMS5951B:2023 Nickel Alloy, Corrosion- and Heat-Resistant, Sheet, Strip, and Plate 57Ni - 20Cr - 10Co - 8.5Mo - 2.1Ti - 1.5Al - 0.005B Vacuum Induction and Consumable Electrode Melted, Solution Heat Treated Precipitation Heat Treatable
SAE AMS5401C:2004(R2023) Nickel Alloy, Corrosion- and Heat-Resistant, Investment Castings 62Ni - 21.5Cr - 9.0Mo - 3.6Cb (Nb) Vacuum Melted, Vacuum Cast As Cast

View more information
£94.27
Excluding VAT

Access your standards online with a subscription

Features

  • Simple online access to standards, technical information and regulations.

  • Critical updates of standards and customisable alerts and notifications.

  • Multi-user online standards collection: secure, flexible and cost effective.